GRANULED ELECTROPORCELAIN CLAY ESC7 (1280°C)
GRANULED ELECTROPORCELAIN CLAY ESC7 (1280°C)

ESC7 ELECTROPORCELAIN CASTING SLIP 

For one firing :1280 °C.

If it is gonna fire twice :

Bisque Firing : 900 - 950 °C

Glazed Firing : 1180 - 1200 °C 

Physical Condition : Powder - Granuled (There is no other form)

Should be mixed with sodium silicate about 0,1 % for hardening.

Available for casting or pressing processes.

Packing  : 12,5 - 25 Kg.

Pallet Dimension of 1 ton : 100*120*80 cm.

CHEMICAL ANALYSIS

Si02   Ah03  Fe203   Ti02  CaO  MgO  Na20  K20  A.Z. 

66,7%

21,5%  0,5%  0,6%  0,3%   0,3%  3,6%   0,4%   6,1%

 

GRAIN SIZE

+60 µm  % 2,30

-20 µm  % 75

-10 µm  % 64

-2 µm  % 42,5 

  

FEATURES

Dry Tensile Strength  = 20 kg/cm2

Shrinkage = % 9 (at 1250 °C)

Fired Color
Creamy
Fireclay Content
Not Contains
First Firing (Bisque)
950 - 970°C
Second Firing (Glazed)
1180 - 1200 °C
Package
25 KG.
Package Type
Sack